MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Niagara LaSalle 1018 Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: This low carbon steel has good case hardening properties. Although not classed as a screw machine steel, at times it may be specified. This is an excellent steel for bending and cold forming, with good brazing and welding properties.

Information provided by Niagra LaSalle Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 126
Tensile Strength 64000 psi
Tensile Strength, Yield 54000 psi
Elongation at Break >= 15 %2"
Reduction of Area 40 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.15 - 0.20 %
Iron, Fe 97.65 - 99.1 %as balance
Manganese, Mn 0.60 - 0.90 %
Phosphorus, P <= 0.40 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
302 Stainless Steel, after cold work
302 Stainless Steel, annealed bar
AISI 4140 Steel, oil quenched, 650°C (1200°F) temper, 25 mm (1 in.) round

NNIAL006 / 160296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.