MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® ST329 Polyester Film, 1000 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: MELINEX® ST329 has good handling properties and a unique pearlescent appearance with no pre-treatments. It is heat stabilized for applications in high temperature processes where film registration is critical.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D1505-85
Brightness 95.0 %Whiteness; ASTM E313-79
Thickness 10.0 mil
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction, Static 0.32ASTM D1894
Film Tensile Strength at Break, MD 19000 psiASTM D882A
Film Tensile Strength at Break, TD 24000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 0.10 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.050 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Optical Density 1.2ASTM D1003
Transmission, Visible 6.7 %TLT; ASTM D1003
 
Descriptive Properties
Color0a
 -0.4b
 96.9L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge
DuPont Teijin Films Melinex® S Polyester Film, 48 Gauge
DuPont Teijin Films Melinex® RFL1 Polyester Film, 600 Gauge
DuPont Teijin Films Melinex® HS2 Polyester Film
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge

PDTZ9230 / 139558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.