MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® ST328 is an exceptionally white, opaque film with a satin finish. It is pretreated on both surfaces to promote adhesion to a wide range of solvent-based and UV-curable graphics inks and varnishes, silver conducting inks and dielectrics, and has been heat stabilized to give excellent dimensional stability at temperatures up to 302°F.

Typical Applications: Melinex® ST328 has been developed for use in screen-printed medical test strips where a white background appearance is required. The tight thickness control of this film ensures reliable insertion into reading devices.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D1505-85
Brightness 85.0 %85.0 %Whiteness; ASTM E313-79
Thickness 356 microns14.0 mil
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction, Dynamic 0.400.40A-B; ASTM D1894
Film Tensile Strength at Break, MD 152 MPa22000 psiASTM D882A
Film Tensile Strength at Break, TD 165 MPa24000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C
@Temperature 20.0 - 50.0 °C
10.6 µin/in-°F
@Temperature 68.0 - 122 °F
Melting Point 255 - 260 °C491 - 500 °FASTM E794-85
Shrinkage, MD <= 0.20 %
@Temperature 150 °C,
Time 1800 sec
<= 0.20 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD <= 0.10 %
@Temperature 150 °C,
Time 1800 sec
<= 0.10 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Gloss 45 %45 %60°; ASTM D1003
Yellow Index -1.50 %-1.50 %ASTM D1925
Transmission, Visible 1.1 %1.1 %TLT; ASTM D1003
 
Descriptive Properties
Color-0.1a
 -0.8b
 96.8L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge
DuPont Teijin Films Melinex® D316 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® CORE 2 Polyester Film
DuPont Teijin Films Melinex® HS2 Polyester Film
DuPont Teijin Films Melinex® RFL1 Polyester Film, 600 Gauge

PDTZ9229 / 139557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.