MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Johnson Matthey Argo-braze™ 60V Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Argo-braze™ 60 is a specialized cadmium free and zinc free silver brazing filler metal which makes it suitable for flux-less brazing in reducing or inert gas atmospheres as well as vacuum.

This filler metal is also available as vacuum tube grade material with low and controlled levels of volatile impurities in which case it is designated Argo-braze™ 60V.

Being zinc free the alloy is suitable for the brazing of components in applications where dezincification of zinc containing filler metals might occur, such as exposure to salt water.

The tin content of this filler metal depresses the melting temperature and improves its wetting on ferrous parent metals over the silver-copper filler metal Argo-braze™ 72V. It is, however, prone to liquate (separate into low and high melting constituents) if it is heated slowly through its melting range. For this reason rapid heating methods should be employed wherever possible.

Joint gaps should be between 0.075mm and 0.2mm at brazing temperature.

This filler metal was formerly called RTSN™.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 600 - 730 °C
Solidus 600 °C
Liquidus 730 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 30 %
Silver, Ag 60 %
Tin, Sn 10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Argo-braze™ 502 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 56 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 60 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 61V Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 632 Silver Brazing Filler Metal

NJMMJ9710 / 186111

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.