MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Johnson Matthey Argo-braze™ 632 Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Argo-braze™ 632 is a specialized silver-copper-tin-nickel brazing filler metal. It is used principally for brazing stainless steel joints or joints between stainless steel and another parent material that will be subject to attack in service by interfacial corrosion, commonly called crevice corrosion.

Where a joint involving a stainless steel member will be exposed to damp or wet aqueous based service environments the joint will be susceptible to interfacial corrosion, a unique and rapid form of corrosive attack. The name interfacial corrosion is derived from the failure mechanism, which involves the corroding away of the bonding layer (the interface layer) created between the filler metal and the parent material. It is common for joints that have failed due to interfacial corrosion to show a complete separation of the filler metal from the parent material and this can occur within a period as short as 3 months for immersed joints.

Argo-braze™ 632 has a long melting range and high brazing temperature (691 - 802°C) and flows relatively poorly when molten. It is useful as a gap-filling alloy producing large fillets. Argo-braze™ 632 is an alternative to the Argobraze ™ 56 filler metal, but the lower brazing temperature of the latter makes it easier to use in many applications.

Argo-braze™ 632 does not contain zinc and is hence resistant to dezincification in salt water or marine environments. Typical joint gaps at brazing temperature should be 0.1-0.25mm.

Argo-braze™ 632 is used principally for brazing joints involving a stainless steel member in conditions where interfacial corrosion is likely to be a service hazard. It has been found to offer near complete protection from interfacial corrosion on 300 series austenitic stainless steels, while offering a very high level of protection on the martensitic 403,410, 440A grades and the ferritic 430 grade. Applications might include medical or surgical instruments, steam turbine blades and specialized stainless steel pipework.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 691 - 802 °C1280 - 1480 °F
Solidus 691 °C1280 °F
Liquidus 802 °C1480 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 28.5 %28.5 %
Nickel, Ni 2.5 %2.5 %
Silver, Ag 63 %63 %
Tin, Sn 6.0 %6.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey Argo-braze™ 56 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 502 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 60 Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 60V Silver Brazing Filler Metal
Johnson Matthey Argo-braze™ 61V Silver Brazing Filler Metal

NJMMJ9719 / 186120

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.