MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical KEYFLEX BT 1155D Ester Type TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Description: Injection Molding, TPC-ET, General Purpose, Medium Modulus

Application: Cable & Wire Jackets, Hose & Tubing, Sheet

CAS: 37282-12-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Molecular Weight 458.458 g/mol
Maximum Moisture Content 0.010Injection Molding
 0.010Extrusion Molding
Linear Mold Shrinkage, Flow 0.010 - 0.014 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ASTM D2240
Tensile Strength at Break 34.3 MPa
@Thickness 2.00 mm
50mm/min; ASTM D638
Elongation at Break 550 %
@Thickness 2.00 mm
50mm/min; ASTM D638
Flexural Modulus 1700 kg(f)/cm²
@Thickness 6.40 mm
15mm/min; ASTM D790
Izod Impact, Notched 20.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature -40.0 °C
ASTM D256
 NB
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
Tear Strength 150 kg(f)/cm50mm/min, at Break; ASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmASTM D257
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
ASTM D149
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 °CPeak
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 200 - 240 °CInjection Molding
Middle Barrel Temperature 210 - 230 °CInjection Molding
Front Barrel Temperature 220 - 240 °CInjection Molding
Nozzle Temperature 220 - 240 °CInjection Molding
Zone 1 200 - 220 °CExtrusion Molding
Zone 2 210 - 230 °CExtrusion Molding
Zone 3 215 - 235 °CExtrusion Molding
Zone 4 220 - 240 °CExtrusion Molding
Adapter Temperature 220 - 240 °CExtrusion Molding
Die Temperature 210 - 250 °CExtrusion Molding
Melt Temperature 200 - 240 °CInjection Molding
 200 - 240 °CExtrusion Molding
Mold Temperature 20.0 - 40.0 °CInjection Molding
Drying Temperature 80.0 - 90.0 °CInjection Molding
 80.0 - 90.0 °CExtrusion Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 3.00 - 4.00 hourExtrusion Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Maxxam™ DP-8463-7001 Polypropylene Homopolymer (PP Homopolymer)
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Delrin Delrin® 100T NC010 POM-I
Celanese Hytrel® 5555HS TPC-ET
LG Chemical KEYFLEX BT 1163D Ester Type TPE

PLAY431 / 148441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.