MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Delrin Delrin® 100T NC010 POM-I
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Toughened High Viscosity Acetal Homopolymer

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Water Absorption 0.90 %
@Thickness 2.00 mm
0.90 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.300 %
@Thickness 2.00 mm
0.300 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inISO 294-4, 2577
Melt Flow  1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric; ISO 1133
 2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5959ISO 2039-2
Hardness, Rockwell R 113113ISO 2039-2
Tensile Strength, Yield 55.0 MPa7980 psiISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527-1/-2
Elongation at Yield 25 %25 %ISO 527-1/-2
Tensile Modulus 1.90 GPa276 ksiISO 527-1/-2
Flexural Strength 52.0 MPa
@Strain 3.5 %
7540 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 1.70 GPa247 ksiISO 178
Poissons Ratio 0.410.41
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.60 J/cm²
@Temperature 23.0 °C
12.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+14 ohm-cm6.00e+14 ohm-cmIEC 62631-3-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 42.0 mm/min
@Thickness 1.00 mm
1.65 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °FOptimum, Extrusion
 195 - 205 °C383 - 401 °FRange, Extrusion
 200 - 210 °C392 - 410 °FRange, Injection
 205 °C401 °FOptimum, Injection
Mold Temperature 50.0 °C122 °FOptimum, Injection
 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 80.0 °C176 °FExtrusion
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hourExtrusion, Dehumidified Dryer
 4.00 - 8.00 hour4.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.050 %<= 0.050 %Extrusion
 <= 0.050 %<= 0.050 %Injection
Hold Pressure 60.0 - 80.0 MPa8700 - 11600 psiInjection
 80.0 MPa11600 psiInjection
Annealing Temperature 160 °C320 °FOptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)7E-08
Emissions (mg/kg)<8VDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>POM-I<ISO 11469
PolymerPOM
Processing Hold Pressure Time (s/mm)7.5Injection
Resin IdentificationPOM-IISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shinkong Synthetic Fibers Shinite® D201 PBT
Granite
Delrin Delrin® 100 NC010 POM
Aluminum, Al
Akro-Plastic Akrotek® PK-HM (4773) PK Dry

PDSX5093 / 197733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.