MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Freudenberg N475 Nitrile Elastomer (NBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Key Words: CHEMIGUM® , HYCAR® , PARACRIL® , PERBUNAN®, KRYNAC®, NYSYSN®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73Original Property; ASTM D2240
 69ASTM IRM 903 Oil Immersion, 70 hours; ASTM D2240
 76ASTM #1 Oil Immersion, 70 hours; ASTM D2240
 77Air age, 70 hours; ASTM D2240
Tensile Strength, Ultimate 18.7 MPaOriginal Property; ASTM D412 Die C
 11.407 MPaASTM IRM 903 Oil Immersion, 70 hours; ASTM D412 Die C
 15.147 MPaASTM #1 Oil Immersion, 70 hours; ASTM D412 Die C
 20.009 MPaAir age, 70 hours; ASTM D412 Die C
Elongation at Break 195 %Original Property; ASTM D412 Die C
 130.65 %ASTM IRM 903 Oil Immersion, 70 hours; ASTM D412 Die C
 152.1 %ASTM #1 Oil Immersion, 70 hours; ASTM D412 Die C
 165.75 %Air age, 70 hours; ASTM D412 Die C
Compression Set 5.2 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395 Method B
 
Descriptive Properties
Volume Change (%), ASTM D471-0.9ASTM #1 Oil Immersion, 70 hours at 150°C
 14.3ASTM IRM 903 Oil Immersion, 70 hours at 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Freudenberg N470 Hydrocarbon Elastomer Nitrile
Freudenberg N442 Nitrile Elastomer (NBR)
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Freudenberg N431 Nitrile Elastomer (NBR)
Freudenberg N466 Nitrile Elastomer (NBR)

PSIMR137 / 79099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.