MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Freudenberg N431 Nitrile Elastomer (NBR)  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Key Words: CHEMIGUM® , HYCAR® , PARACRIL® , PERBUNAN®, KRYNAC®, NYSYSN®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060Original Properties; ASTM D2240
 5050ASTM Reference Fuel B Immersion, 70 hours; ASTM D2240
 6161ASTM Fuel A Immersion, 70 hours; ASTM D2240
 6363Air Aging, 70 hours; ASTM D2240
 6363ASTM IRM-903 Oil Immersion, 70 hours; ASTM D2240
 6464Water Resistance, 70 hours; ASTM D2240
Tensile Strength, Ultimate 12.9 MPa1870 psiOriginal Properties; ASTM D412 Die C
 7.4304 MPa1077.7 psiASTM Reference Fuel B Immersion, 70 hours; ASTM D412 Die C
 13.18 MPa1912 psiASTM Fuel A Immersion, 70 hours; ASTM D412 Die C
 13.66 MPa1981 psiAir Aging, 70 hours; ASTM D412 Die C
 15.82 MPa2294 psiASTM IRM-903 Oil Immersion, 70 hours; ASTM D412 Die C
Elongation at Break 486 %486 %Original Properties; ASTM D412 Die C
 292 %292 %ASTM Reference Fuel B Immersion, 70 hours; ASTM D412 Die C
 379.08 %379.08 %Air Aging, 70 hours; ASTM D412 Die C
 448 %448 %ASTM IRM-903 Oil Immersion, 70 hours; ASTM D412 Die C
 476.28 %476.28 %ASTM Fuel A Immersion, 70 hours; ASTM D412 Die C
Compression Set 13 %
@Temperature 100 °C,
Time 79200 sec
13 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395
 
Descriptive Properties
Volume Change (%), ASTM D471-1.1ASTM IRM-903 Oil Immersion, 70 hours at 100°C
 -1.2ASTM Fuel A Immersion, 70 hours at 23°C
 17.1ASTM Reference Fuel B Immersion, 70 hours at 23°C
 -4.8Water Resistance, 70 hours at 100°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg B500 Commercial Nitrile Rubber
Freudenberg N442 Nitrile Elastomer (NBR)
Trelleborg B573 Nitrile Rubber
Freudenberg N470 Hydrocarbon Elastomer Nitrile
Freudenberg N475 Nitrile Elastomer (NBR)

PSIMR140 / 79102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.