MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TELC-1000-105 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: High Hardness; Low Density; Low Flow; Low Specific Gravity; Without Fillers

Uses: General Purpose; Industrial Applications

Agency Rating: UL 94

RoHS Compliant:RoHS Compliant

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.892 g/ccASTM D792
Viscosity 378 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59
@Time 5.00 sec
ASTM D2240
 62.2
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Change in Air
Tensile Strength at Break 1940 psiAcross Flow; ASTM D412
 2310 psiFlow; ASTM D412
Tensile Strength 1630 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
 1650 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain 1600 psi
@Strain 100 %
Across Flow; ASTM D412
 1900 psi
@Strain 100 %
Flow; ASTM D412
Elongation at Break 230 %Flow; ASTM D412
 290 %Across Flow; ASTM D412
 191 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Change in Air; ISO 188
 235 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Change in Air; ISO 188
Tear Strength 691 pliAcross Flow, Die C; ASTM D624
Compression Set 54 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D695
 74 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D695
 93 %
@Temperature 90.0 °C,
Time 252000 sec
ASTM D695
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -67.0 °FASTM D746
UL RTI, Electrical 122 °FUL 746
UL RTI, Mechanical with Impact 122 °FUL 746
UL RTI, Mechanical without Impact 122 °FUL 746
Flammability, UL94 HB
@Thickness 0.762 mm
All Colors
 
Processing PropertiesOriginal ValueComments
Processing Temperature 370 - 410 °FInjection, Melt
Rear Barrel Temperature 340 - 380 °FInjection
Middle Barrel Temperature 350 - 390 °FInjection
Front Barrel Temperature 360 - 400 °FInjection
Nozzle Temperature 370 - 410 °FInjection
Zone 1 330 - 370 °FExtrusion
Zone 2 340 - 380 °FExtrusion
Zone 3 350 - 390 °FExtrusion
Zone 5 360 - 400 °FExtrusion
Die Temperature 374 - 410 °FExtrusion
Mold Temperature 77.0 - 150 °FInjection
Drying Temperature 176 °F
Dry Time 2.00 hour
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1630 / 238121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.