MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay FM® 99 Surfacing Film
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 99 is a modified epoxy-based adhesive film designed for surfacing composite structures. It provides a high quality, ready-to-paint surface finish with no core mark off. Its 250°F/350°F (121°C/177°C) dual cure capability makes FM 99 surfacing film suitable for surfacing a wide variety of composite prepregs and materials. FM 99 surfacing film is supplied as a thin film with a random mat carrier. It can also be supplied unsupported or with various copper, aluminum and other metallic screens and foils for lightning strike applications.

Features & Benefits:

  • 250°F/350°F (121°C/177°C) dual cure capability
  • Provides a high quality, ready-to-paint surface finish with no core mark off
  • Prevents moisture ingression into the composite structure by eliminating the surface porosity
  • Can be combined with lightning strike screen or foil materials for lightning strike applications
Applications:
  • Metal-to-metal bonding
  • Composite-to-composite bonding
  • Composite-to-metal bonding

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 18.6 MPa2700 psiLap, Cure 60 mins at 121°C
 22.8 MPa3300 psiLap, Cure 60 mins at 177°C
 23.68 MPa3435 psiLap, Bagged film held for 6 months at 75°F (24°C)
 24.0 MPa3480 psiLap, Bagged film held for 4 months at 75°F (24°C)
 24.8 MPa3600 psiLap, Bagged film held for 2 months at 75°F (24°C)
 24.1 MPa
@Temperature 24.0 °C
3490 psi
@Temperature 75.2 °F
Initial Lap
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorDark Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay FM® 73U Epoxy Film Adhesive
Solvay FM® 94U Adhesive Film
Solvay FM® 300-2K Film Adhesive, psf 0.1 (489 gsm)
Solvay FM® 300 Epoxy Film Adhesive
Overview of materials for Epoxy Adhesive

PCYTED050 / 180352

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.