MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film and chemical resistance properties. The low residual emulsifier level provides good end product performance in the areas of clarity, moisture blush resistance and low taste and odor. Geon® 171 is accepted by FDA for use under 21CFR175.300, food contact application.

Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® STP 1434 (formulation): 100phr Geon® 171, 55phr Aromatic100, 20phr Drapex 334-F, 5phr ESO, and 3phr Therm-Chek SP 120 LOHF

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Bulk Density 0.272 g/cc
Fineness 5.5Hegman, North Fineness; Geon® STP 1434
Relative Viscosity 3.04 cPCorrelation, Cyclohexanone 1%; Internal Method
Brookfield Viscosity 175 cPOne Hour Viscosity @ 30 rpm Geon® STP 1434 (with provided formulation); Internal Method
 200 cPOne Day Viscosity @ 30 rpm Geon® STP 1434 (with provided formulation); Internal Method
 300 cPOne Hour Viscosity @ 6 rpm Geon® STP 1434 (with provided formulation); Internal Method
 375 cPOne Day Viscosity @ 6 rpm Geon® STP 1434 (with provided formulation); Internal Method
Viscosity Measurement 1.4Inherent; ASTM D1243-60-A
 
Processing PropertiesOriginal ValueComments
Moisture Content 0.090 %Karl FisherGeon® STP 683; Internal Method
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Clean Point5.25 HegmanInternal Method; Grind, Geon® STP 1434 (with provided formulation)
FeaturesLow to No Odor
 Low to No Taste
 Ultra High Molecular Weight
FormsPowderFine, white powder
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value82No Standard; Correlation, 0.5g/100ml
Methanol Extractables1.3%Internal Method; Geon® STP 894
Polymerization ProcessEmulsion
Processing MethodCasting
 Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Residual Vinyl Chloride Monomer< 1 ppmInternal Method; Geon® STP 1005
UsesCoating Applications
 Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 170 Series 179 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 170 Series 178 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

PH0POL1442 / 146011

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.