MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions 170 Series 179 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940. Note: The values set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Fineness 5.05.0North Fineness; Geon® 390
Apparent Bulk Density 0.320 - 0.400 g/cc0.0116 - 0.0145 lb/in³ASTM D1505
Relative Viscosity 2.71 cP2.71 cP1% Cyclohexanone
Brookfield Viscosity 2.6 cP2.6 cPInitial, V12, Geon® 1010
 3.6 cP3.6 cPOne Day, V12, Geon® 1010
Viscosity Measurement 1.21.2Inherent; ASTM D1243-60-A
Melt Flow 270 g/10 min
@Pressure 0.655 MPa
270 g/10 min
@Pressure 95.0 psi
Severs Efflux; Geon® 1010
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 17.9 MPa2600 psiOptimum; FF; ASTM D638
Elongation at Yield 350 %350 %FF; Optimum Tensile; ASTM D412
 
Optical PropertiesMetricEnglishComments
Gloss 91 %91 %60°, FF, ALTC-65
Transmission, Visible 88 %88 %FF, ATLC-66
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.050 %0.050 %Karl Fisher-Geon® 683
 
Descriptive Properties
Degree of Polymerization1750Correlation
FeaturesHigh Molecular Weight
 Resilient
FormsPowder
Gel Temperature95 °CFF, ALTC-29
Generic MaterialPVC Homopolymer
Generic NamePolyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value77No Standard; Correlation
Methanol Extractables1.3%Geon® 894
Polymerization ProcessDispersion
Processing MethodCasting
 Dip Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesCoating Applications
 Protective Coatings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 170 Series 178 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® Performance Solutions 180 Series 180X5 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

PH0POL0869 / 145438

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.