MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Impet® Hi430 15% Glass Filled, Impact Modified PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Description: Impet Hi 430 is a 15% glass filled and impact modified PET which has an excellent balance of mechanical properties as well as excellent processability and surface appearance.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccISO 1183 & ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 73.0 MPa5 mm/min; ISO 527-2/1A
 9800 psiASTM D638
Elongation at Break 3.0 %5 mm/min; ISO 527-2/1A
Tensile Modulus 4.80 GPa1 mm/min; ISO 527-2/1A
 620000 psiASTM D638
Flexural Strength 115 MPaISO 178
Flexural Yield Strength 16000 psiASTM D790
Flexural Modulus 4.20 GPaISO 178
 530000 psiASTM D790
Izod Impact, Notched 3.40 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 18.0 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²ISO 180/1U
Charpy Impact Unnotched 5.30 J/cm²ISO 179/1eU
 3.80 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²ISO 179/1eA
 0.840 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 490 V/milShort Term; ASTM D149
Arc Resistance 120 secASTM D495
Comparative Tracking Index 400 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-2
Melting Point 250 °CISO 11357-1,2,3
Deflection Temperature at 0.46 MPa (66 psi) 236 °CISO 75-1, -2
 433 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 270 °C
Middle Barrel Temperature 270 - 280 °C
Front Barrel Temperature 280 - 285 °C
Nozzle Temperature 270 - 290 °C
Melt Temperature 270 - 290 °C
Mold Temperature 130 °C
Back Pressure 80.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hippe PET Polyethylene Terephthalate
GEHR Plastics PET Polyethylene Terephthalate
Indorama AlphaPet Preformance® 1708CC(A) PET Resin
Indorama AlphaPet Preformance® 1708HS(A) PET Resin
Indorama Auriga Polymers Invista™ Polyclear™ Crystal™ 3302 PET Resin

PHCW57 / 45998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.