MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Indorama AlphaPet Preformance® 1708HS(A) PET Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Description: Preformance® PET 1708HS(A) is a food grade PET copolymer that is suitable for a wide variety of beverage and juice containers hot fill application, high temperature filling. Offers exceptional clarity and color and is engineered for heat-set. The low acetaldehyde content in the resin helps eliminate any impact on aroma and flavor. Preformance® PET 1708HS(A) resin is considered safe for food packaging applications based upon compliance with FDA Regulation 21 CFR Section 177.1630 specifications.

Key Words: Exceptional clarity and color
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.817 - 0.881 g/cc0.0295 - 0.0318 lb/in³QCL-03-0004
Viscosity Test 78 - 82 cm³/g0.78 - 0.82 dl/gIntrinsic; QCL-03-0015
 
Chemical PropertiesMetricEnglishComments
Acetaldehyde <= 2.00 ppm<= 2.00 ppmQCL-03-0001
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.25 %<= 0.25 %as packed, QCK-03-0011
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Color, CIE> 78 (L)QCL-03-0009
 -4.0 to 1.0 (b)QCL-03-0009
Contaminants/Black SpecsNoneQCL-03-0028
Dust<300 ppmas packed, QCL-03-0014
ProcessBlow Molding
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indorama AlphaPet Preformance® 1708CC(A) PET Resin
Hippe PET Polyethylene Terephthalate
Indorama AlphaPet Preformance® ES11(A) PET Resin
Celanese Impet® Hi430 15% Glass Filled, Impact Modified PET
GEHR Plastics PET Polyethylene Terephthalate

PINDOA902 / 126376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.