MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pyrite N-14 Refractory Board
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrotek N-14 is a fiberglass reinforced calcium silicate board specifically developed for the non-ferrous industry. The superior strength and unique formulation of Pyrotek N-14 makes it the preferred material for precision machined parts. Our machine shops are equipped with CNC tooling equipment to produce complex components to customer specifications.

Applications

  • Dip tubes
  • Pouring spouts
  • Hot-top rings
  • Stopper pins
  • End dams
  • Floats
  • Launders

Advantages

  • Asbestos-free
  • Low thermal conductivity
  • Resistant to thermal shock
  • Non-wetting
  • Excellent machining characteristics

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.840 g/cc
Loss On Ignition <= 8.0 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00700 GPa
Compressive Strength 17.0 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.00 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.120 W/m-K
@Temperature 200 °C
 0.121 W/m-K
@Temperature 300 °C
 0.123 W/m-K
@Temperature 100 °C
 0.125 W/m-K
@Temperature 400 °C
Maximum Service Temperature, Air 850 °CContinuous
Shrinkage 0.49 %
@Temperature 1000 °C,
Time 86400 sec
Linear
 3.5 %
@Temperature 1000 °C,
Time 86400 sec
Thickness
 
Descriptive Properties
Screw Grip (Pull) Penetration Depth110 kg19 mm
 115 kg22 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek F-51 Dense Machinable Board
Pyrotek O'-Sialon Non-Oxide Ceramic
Pyrotek Valcor® G Pre-Cast Shapes
Pyrotek Valcor® G-AZ Pre-Cast Shapes
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems

CPYRO041 / 1803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.