MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are formed to near net size.

Applications

  • Trough liners and launders
  • Distribution pan linings
  • Tundishes and pouring basins
  • Hot top casting components

Advantages

  • Excellent insulating properties
  • Light-weight and low density
  • Excellent resistance to molten aluminum
  • Good erosion resistance
  • Highly resistant to thermal shock
  • No preheating required
  • Easy to install and maintain

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.625 - 0.657 g/cc0.0226 - 0.0237 lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0700 W/m-K
@Temperature 295 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 563 °F
 0.110 W/m-K
@Temperature 540 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.170 W/m-K
@Temperature 815 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 1500 °F
Maximum Service Temperature, Air 1150 °C2100 °F
Shrinkage  0.60 %
@Temperature 760 °C,
Time 86400 sec
0.60 %
@Temperature 1400 °F,
Time 24.0 hour
Permanent Linear Change
 1.2 %
@Temperature 870 °C,
Time 86400 sec
1.2 %
@Temperature 1600 °F,
Time 24.0 hour
Permanent Linear Change
 2.4 %
@Temperature 980 °C,
Time 86400 sec
2.4 %
@Temperature 1800 °F,
Time 24.0 hour
Permanent Linear Change

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek O'-Sialon Non-Oxide Ceramic
Pyrotek F-51 Dense Machinable Board
Pyrotek Valcor® G Pre-Cast Shapes
Pyrotek Valcor® G-AZ Pre-Cast Shapes
Pyrotek O-1 Low-Temperature Felt

CPYRO145 / 1866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.