MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: High Hydrolysis resistance and good crystallinity. Suggested for injection molding.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Linear Mold Shrinkage 0.011 in/inASTM D995
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength at Break 54.0 MPaDIN 53504
Elongation at Break 610 %ASTM D412
100% Modulus 0.0204 GPa
@Strain 100 %
DIN 53504
300% Modulus 0.0326 GPa
@Strain 300 %
DIN 53504
Rebound 34 %Bayshore; ASTM D2632
Tear Strength 1250 pliASTM D624
Abrasion 30[mm3]; ISO 4649
Compression Set 44 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 56 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 205 - 215 °CHuntsman/TMA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Taiwan Sheen Soon Sheenthane® D6010 Thermoplastic Polyurethane Elastomer
Taiwan Sheen Soon Sheenthane® D6610 Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester

PHU9906 / 150366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.