MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: High Hydrolysis resistance and good crystallinity. Suggested for injection molding.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inASTM D995
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength at Break 54.0 MPa7830 psiDIN 53504
Elongation at Break 610 %610 %ASTM D412
100% Modulus 20.4 MPa
@Strain 100 %
2960 psi
@Strain 100 %
DIN 53504
300% Modulus 32.6 MPa
@Strain 300 %
4730 psi
@Strain 300 %
DIN 53504
Rebound 34 %34 %Bayshore; ASTM D2632
Tear Strength 219 kN/m1250 pliASTM D624
Abrasion 3030[mm3]; ISO 4649
Compression Set  44 %
@Temperature 23.0 °C,
Time 252000 sec
44 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 56 %
@Temperature 70.0 °C,
Time 86400 sec
56 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 205 - 215 °C401 - 419 °FHuntsman/TMA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Taiwan Sheen Soon Sheenthane® D6010 Thermoplastic Polyurethane Elastomer
Taiwan Sheen Soon Sheenthane® D6610 Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester

PHU9906 / 150366

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.