MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M S42XHS Glass Bubbles
Categories: Ceramic; Glass

Material Notes: 3M™ Glass Bubbles S42XHS are high-strength additives for polymers made from a water-resistant and chemically stable sodalime-borosilicate glass. These hollow glass microspheres can be compounded with a variety of polymers to reduce the overall thermal conductivity of the composite. These composites can be coated or incorporated into deep sea oil pipelines to improve the flow assurance properties of the system. The high strength of S42XHS glass bubbles can withstand both the high processing pressure of polymer extrusion and the pressure of seawater in many applications. The S42XHS glass bubbles have isostatic crush strengths of 8000 psi with a minimum of 90% survival.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.420 g/ccTrue
Volatiles 0.50 %
Particle Size 22 µmAverage diameter
pH 9.55% loading in water
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 8000 psi90% survival by volume
 8000 psi90% survival by volume
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.140 W/m-K
@Temperature 50.0 °C
Softening Point 600 °C
 
Descriptive Properties
Alkalinity0.5 milliequivalents/gram
AppearanceWhite, powderyunaided eye
CompositionSoda-lime-borosilicate glass
Flotation97.5%density <1.0 g/cc
Packing factor60%bulk
ShapeHollow spheres with thin walls

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M S38HS Glass Bubbles
3M iM30K Glass Bubbles
3M iM16K Glass Bubbles
3M HGS8000X Glass Bubbles
3M HGS6000 Glass Bubbles

CMM33072 / 167819

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.