MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M iM16K Glass Bubbles
Categories: Ceramic; Glass

Material Notes: 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding applications. These low-density particles are used in a wide range of industries to reduce part weight, lower costs and enhance product properties. The unique spherical shape of 3M glass bubbles offers a number of important benefits, including: higher filler loading, lower viscosity/improved flow and reduced shrinkage and warpage. It also helps the 3M glass bubbles blend readily into compounds and makes them adaptable to a variety of production processes including spraying, casting and molding. The chemically stable soda-lime-borosilicate glass composition of 3M glass bubbles provides excellent water resistance to create more stable emulsions. They are also non-combustible and nonporous, so they do not absorb resin. And, their low alkalinity gives 3M glass bubbles compatibility with most resins, stable viscosity and long shelf life.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.430 - 0.490 g/cc0.0155 - 0.0177 lb/in³
 0.460 g/cc0.0166 lb/in³
Volatiles 0.50 %0.50 %
Particle Size 12 µm12 µm10th%
 20 µm20 µm50th%
 30 µm30 µm90th%
 40 µm40 µmEffective Top Size
pH 9.59.5at 5 wt% loading in water
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 110 MPa16000 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.2 - 1.7
@Frequency 1e+8 Hz
1.2 - 1.7
@Frequency 1e+8 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.153 W/m-K1.06 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 600 °C1110 °F
Softening Point 600 °C1110 °F
 
Descriptive Properties
Alkalinity<0.5 milliequivalents/gram
AppearanceWhiteunaided eye
Chemical Resistancesoda-lime-borosilicate glass
Flotation96%density <1.0 g/cc
Oil Absorption0.2-0.6 g oil/100 ccASTM D1483
Packing factor60%bulk density to true particle density
ShapeHollow spheres with thin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M S38HS Glass Bubbles
3M iM30K Glass Bubbles
3M S60 Glass Bubbles
3M S60HS Glass Bubbles
3M HGS5000 Glass Bubbles

CMM33070 / 167817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.