MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoset Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 3.80 g/ccAverage value: 1.87 g/cc Grade Count:612
Oxygen Transmission 98.0 - 150 cc-mm/m²-24hr-atmAverage value: 105 cc-mm/m²-24hr-atm Grade Count:40
Viscosity 1.50 - 300 cPAverage value: 89.8 cP Grade Count:7
 20.0 - 180 cP
@Temperature 60.0 - 121 °C
Average value: 56.8 cP Grade Count:14
Mooney Viscosity 3.00 - 200Average value: 55.2 Grade Count:490
Molecular Weight 3000 g/molAverage value: 3000 g/mol Grade Count:3
Evaporation Loss 2.00 - 2.00 %
@Temperature 200 - 200 °C
Average value: 2.00 % Grade Count:3
 2.00 - 2.00 %
@Time 7200 - 7200 sec
Average value: 2.00 % Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 38.0 - 100Average value: 73.6 Grade Count:971
 35.0 - 85.0
@Temperature 225 - 225 °C
Average value: 71.4 Grade Count:1
 45.0 - 96.0
@Temperature 60.0 - 275 °C
Average value: 71.4 Grade Count:37
 45.0 - 96.0
@Time 252000 - 3.63e+6 sec
Average value: 71.4 Grade Count:37
Hardness, Shore D 47.0 - 80.0Average value: 59.8 Grade Count:4
Hardness, Shore M 72.0 - 83.0Average value: 80.0 Grade Count:4
Tensile Strength, Ultimate 0.750 - 160 MPaAverage value: 14.6 MPa Grade Count:919
 17.24 - 20.68 MPa
@Temperature 225 - 225 °C
Average value: 13.4 MPa Grade Count:1
 7.00 - 18.104 MPa
@Temperature 60.0 - 275 °C
Average value: 13.4 MPa Grade Count:49
 7.00 - 18.104 MPa
@Time 86400 - 3.63e+6 sec
Average value: 13.4 MPa Grade Count:49
Tensile Strength, Yield 0.600 - 23.0 MPaAverage value: 9.37 MPa Grade Count:225
Elongation at Break 25.0 - 753 %Average value: 224 % Grade Count:1055
 150 - 160 %
@Temperature 225 - 225 °C
Average value: 204 % Grade Count:1
 128.1 - 284.76 %
@Temperature 60.0 - 275 °C
Average value: 204 % Grade Count:48
 128.1 - 284.76 %
@Time 86400 - 3.63e+6 sec
Average value: 204 % Grade Count:48
Modulus of Elasticity 0.0000800 - 0.140 GPaAverage value: 0.0207 GPa Grade Count:30
 0.000480 - 0.000480 GPa
@Temperature 100 - 100 °C
Average value: 0.000480 GPa Grade Count:2
 0.000480 - 0.000480 GPa
@Frequency 1.00 - 1.00 Hz
Average value: 0.000480 GPa Grade Count:2
Flexural Modulus 0.00400 - 0.0170 GPaAverage value: 0.0100 GPa Grade Count:3
Compressive Modulus 0.000300 - 0.0153 GPaAverage value: 0.00534 GPa Grade Count:4
Rebound 5.00 - 40.0 %Average value: 8.86 % Grade Count:11
Poissons Ratio 0.370 - 0.510Average value: 0.494 Grade Count:19
Shear Modulus 0.00193 - 0.0243 GPaAverage value: 0.00760 GPa Grade Count:19
 0.0430 - 0.0430 GPa
@Temperature -12.0 - -12.0 °C
Average value: 0.0430 GPa Grade Count:2
Secant Modulus 0.00512 - 0.0685 GPaAverage value: 0.0215 GPa Grade Count:19
Coefficient of Friction 0.500 - 1.16Average value: 0.791 Grade Count:51
Tear Strength Test 132 - 359Average value: 232 Grade Count:21
Tear Strength 3.06 - 168 kN/mAverage value: 29.8 kN/m Grade Count:129
 5.20 - 10.4 kN/m
@Temperature 150 - 150 °C
Average value: 8.16 kN/m Grade Count:5
Compression Set 3.00 - 91.0 %Average value: 22.7 % Grade Count:1026
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00500 - 5.00e+17 ohm-cmAverage value: 3.02e+16 ohm-cm Grade Count:51
Surface Resistance 2510 - 5.10e+11 ohmAverage value: 2.07e+11 ohm Grade Count:3
Shielding Effectiveness 70.0 - 113 dBAverage value: 98.3 dB Grade Count:3
Dielectric Constant 2.50 - 11.4Average value: 9.75 Grade Count:44
Dielectric Strength 2.60 - 25.0 kV/mmAverage value: 23.3 kV/mm Grade Count:46
Dissipation Factor 0.00260 - 0.0800Average value: 0.0292 Grade Count:6
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 - 570 µm/m-°CAverage value: 263 µm/m-°C Grade Count:71
Specific Heat Capacity 1.65 - 1.67 J/g-°CAverage value: 1.65 J/g-°C Grade Count:40
 0.945 - 1.50624 J/g-°C
@Temperature 50.0 - 150 °C
Average value: 1.12 J/g-°C Grade Count:6
Thermal Conductivity 0.200 - 0.300 W/m-KAverage value: 0.235 W/m-K Grade Count:40
 0.170 - 0.190 W/m-K
@Temperature 50.0 - 200 °C
Average value: 0.180 W/m-K Grade Count:3
Maximum Service Temperature, Air 93.3 - 350 °CAverage value: 236 °C Grade Count:393
Minimum Service Temperature, Air -65.0 - 2.22 °CAverage value: -18.6 °C Grade Count:531
Brittleness Temperature -60.0 - 3.00 °CAverage value: -24.5 °C Grade Count:159
Glass Transition Temp, Tg -51.1 - 10.0 °CAverage value: -18.7 °C Grade Count:180
Transformation Temperature -40.0 - -2.00 °CAverage value: -8.54 °C Grade Count:13
Flash Point 15.6 - 400 °CAverage value: 323 °C Grade Count:93
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.37Average value: 1.37 Grade Count:3
Transmission, Visible 25.0 - 90.0 %Average value: 35.8 % Grade Count:6
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 232 °CAverage value: 203 °C Grade Count:151
Moisture Content 0.500 %Average value: 0.500 % Grade Count:7
Cure Time 0.400 - 4320 minAverage value: 32.1 min Grade Count:78
 0.000 - 1440 min
@Temperature 121 - 290 °C
Average value: 460 min Grade Count:104
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 21.6 %Average value: 21.6 % Grade Count:10
Fluorine, F 57.0 - 73.0 %Average value: 66.8 % Grade Count:340
Oxygen, O 9.40 %Average value: 9.40 % Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Overview of materials for Chlorosulfonated Polyethylene Rubber

O1940 / 77922

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.