MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Eastman DB Acetate Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 124-17-4

Product Description: Eastman™ DB Acetate (Diethylene Glycol Monobutyl Ether Acetate) is a high boiling glycol ether ester widely used in printing inks, high-bake enamels, and as a coalescing aid in low pH latex paints. Eastman™ DB Acetate is especially useful in screen inks and as a retarder solvent in coil coatings. It has application as a selective solvent in the separation of alcohols and ketones by distillation.

Application/Uses:

  • Coatings - Architectural
  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - Consumer Electronics
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Transportation
  • Graphic Arts - Printing Inks
  • Process Solvent
Key Attributes:
  • Efficient coalescent
  • Excellent solvent activity
  • High blush resistance
  • High electrical resistance
  • LVP-VOC
  • Readily biodegradable
  • Slow evaporation rate

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/cc
Viscosity 3.2 cP
Molecular Weight 204.27 g/mol
Vapor Pressure <= 0.0000526 atm
@Temperature 20.0 °C
 <= 0.000197 atm
@Temperature 55.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 20.3 atm
Critical Temperature 407.6 °C
Total Acid Number <= 0.030
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
Melting Point -32.0 °CFreezing Point
Boiling Point 235 °C@ 760 mm Hg, Initial
 250 °C@ 760 mm Hg, Dry Point
Flash Point 105 °CTag Closed Cup
 105 °CCleveland Open Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.43
 
Descriptive Properties
ColorPt-Co
Fire Point128°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5211 / 222405

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.