MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Eastman DB Acetate Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 124-17-4

Product Description: Eastman™ DB Acetate (Diethylene Glycol Monobutyl Ether Acetate) is a high boiling glycol ether ester widely used in printing inks, high-bake enamels, and as a coalescing aid in low pH latex paints. Eastman™ DB Acetate is especially useful in screen inks and as a retarder solvent in coil coatings. It has application as a selective solvent in the separation of alcohols and ketones by distillation.

Application/Uses:

  • Coatings - Architectural
  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - Consumer Electronics
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Transportation
  • Graphic Arts - Printing Inks
  • Process Solvent
Key Attributes:
  • Efficient coalescent
  • Excellent solvent activity
  • High blush resistance
  • High electrical resistance
  • LVP-VOC
  • Readily biodegradable
  • Slow evaporation rate

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³
Viscosity 3.2 cP3.2 cP
Molecular Weight 204.27 g/mol204.27 g/mol
Vapor Pressure  <= 0.0000533 bar
@Temperature 20.0 °C
<= 0.0400 torr
@Temperature 68.0 °F
 <= 0.000200 bar
@Temperature 55.0 °C
<= 0.150 torr
@Temperature 131 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 20.6 bar15400 torr
Critical Temperature 407.6 °C765.7 °F
Total Acid Number <= 0.030<= 0.030
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C55.6 µin/in-°F
Melting Point -32.0 °C-25.6 °FFreezing Point
Boiling Point 235 °C455 °F@ 760 mm Hg, Initial
 250 °C482 °F@ 760 mm Hg, Dry Point
Flash Point 105 °C221 °FTag Closed Cup
 105 °C221 °FCleveland Open Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.431.43
 
Descriptive Properties
ColorPt-Co
Fire Point128°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5211 / 222405

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.