MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M FC-4400 Ionic Liquid Antistatic
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: 3M™ Ionic Liquid Antistatic FC-4400 is a high purity antistatic additive compatible with a variety of high performance polymer systems.

Features and Benefits:

  • Optical Clarity
  • No metal or halogen ions
  • Very low water solubility provides for excellent antistatic durability
  • Static dissipation in wide variety of polymers with typical resistivities of 109 to 1012 ohms/sq
  • Thermal stability with a TGA trigger temperature of 429 C
  • Wide liquid range for ease of handling in production

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/cc
Volatiles <= 0.10 %
pH 5.0neutral
Viscosity 531 cPsupercooled
 
Thermal PropertiesOriginal ValueComments
Melting Point 27.5 °C
 
Descriptive Properties
AppearanceClear colorless liquid or white crystalline solid
Solubility765 ppmin water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M HQ-115IL Ionic Liquid Precursor
Synovial fluid
Enviro Tech International EnSolv® Ionic n-Propyl Bromide Vapor Degreasing Solvent

PMM33124 / 167871

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.