MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M HQ-115IL Ionic Liquid Precursor
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: 3M™ Ionic Liquid Precursor HQ-115IL contains the anion bistrifluoromethanesulfonimide (TFSI) which is useful for manufacture of ionic liquids for a variety of applications including polymer antisats, electrolytes and chemical process solvents.

Features and Benefits:

  • Hydrophobic: Very low solubility in water
  • Lipophilic: Improved solubility in organic polymers
  • Electrolytic, thermal, UV and hydrolytic stability
  • HQ-115IL is an aqueous concentrate for simplified handling and industrial hygiene.
  • HQ-115IL undergoes rapid ion exchange for the manufacture of ionic liquids

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 78 - 82 %78 - 82 %
pH 6.0 - 10.56.0 - 10.5
Viscosity 16.3 - 16.7 cP16.3 - 16.7 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 139.9 °C
@Pressure 0.101 MPa
283.8 °F
@Pressure 14.7 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M FC-4400 Ionic Liquid Antistatic
Synovial fluid
Enviro Tech International EnSolv® Ionic n-Propyl Bromide Vapor Degreasing Solvent

PMM33125 / 167872

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.