MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Stellite Deloro® 208 PM after P/M Processing
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.40 g/ccP/M (98%)
 8.53 g/ccTheoretical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 404Converted from Rockwell C hardness.
 254
@Temperature 760 °C
Converted from Rockwell C hardness
 337
@Temperature 649 °C
Converted from Rockwell C hardness
 373
@Temperature 538 °C
Converted from Rockwell C hardness
Hardness, Knoop 486Converted from Rockwell C hardness.
 299
@Temperature 760 °C
Converted from Rockwell C hardness
 402
@Temperature 649 °C
Converted from Rockwell C hardness
 448
@Temperature 538 °C
Converted from Rockwell C hardness
Hardness, Rockwell A 72Converted from Rockwell C Hardness.
 63
@Temperature 760 °C
Converted from Rockwell C hardness
 69
@Temperature 649 °C
Converted from Rockwell C hardness
 71
@Temperature 538 °C
Converted from Rockwell C hardness
Hardness, Rockwell B 113Converted from Rockwell C Hardness. Beyond the normal Rockwell B range, for comparison only.
Hardness, Rockwell C 44Hot hardness.
 25
@Temperature 760 °C
Hot hardness.
 37
@Temperature 649 °C
Hot hardness.
 41
@Temperature 538 °C
Hot hardness.
Hardness, Vickers 428Converted from Rockwell C hardness.
 261
@Temperature 760 °C
Converted from Rockwell C hardness
 352
@Temperature 649 °C
Converted from Rockwell C hardness
 393
@Temperature 538 °C
Converted from Rockwell C hardness
Tensile Strength, Ultimate 690 MPa
 483 MPa
@Temperature 760 °C
 552 MPa
@Temperature 538 °C
 552 MPa
@Temperature 649 °C
Elongation at Break <= 1.0 %in 25.4 mm
 <= 1.0 %
@Temperature 538 °C
in 25.4 mm
 <= 1.0 %
@Temperature 649 °C
in 25.4 mm
 1.0 %
@Temperature 760 °C
in 25.4 mm
 
Component Elements PropertiesOriginal ValueComments
Boron, B <= 1.0 %
Carbon, C 2.6 %
Chromium, Cr 26 %
Cobalt, Co 10 %
Iron, Fe 12.5 %
Manganese, Mn <= 0.75 %
Molybdenum, Mo 10 %
Nickel, Ni 24 %As Remainder
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
Tungsten, W 10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Deloro® 208 PM cast
Kennametal Stellite Deloro® N-6 PM with P/M Processing
Kennametal Stellite Deloro® 40G
Kennametal Stellite Deloro® 711 PM after P/M Processing
Kennametal Stellite Deloro® 716 PM with P/M Processing

ND208A / 16075

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.