MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Glass fiber Filled; UHMW PE (Ultra High Molecular Weight PE)

Material Notes: The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from the surface give a rounded and hard sliding surface. This material is used for applications that involve manufacturing and transportation at high pressure.

Special Properties:
• Protects the sliding partner
• Extremely good resistance to chemicals
• Approved for use in the food industry (EU and FDA

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PE-UHMW
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 0.940 g/ccISO 1183
Moisture Absorption at Equilibrium <= 0.010 %ISO 62
Water Absorption at Saturation <= 0.010 %ISO 62
Molecular Weight 9.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65DIN 53505
Ball Indentation Hardness 44.0 MPa
Tensile Strength at Break >= 29.0 MPaISO 527
Tensile Strength 25.0 MPaISO 527
Elongation at Break 290 %ISO 527
Modulus of Elasticity 0.700 GPa
Compressive Yield Strength 9.50 MPa
@Strain 1 %
ISO 604
 15.0 MPa
@Strain 2 %
ISO 604
 24.0 MPa
@Strain 5.0 %
ISO 604
Charpy Impact, Notched >= 100 kJ/m²ISO 179
Coefficient of Friction, Dynamic 0.10 - 0.20
Sand Slurry 80value in %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Strength <= 45.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear 170 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.400 W/m-KISO 52612
Melting Point 130 - 135 °CISO 3146
Maximum Service Temperature, Air 90.0 °CShort Term
 80.0 °C
@Time 1.80e+7 sec
Minimum Service Temperature, Air -200 °C
Glass Transition Temp, Tg -120 °C
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorLight Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR™ Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked
Röchling Polystone® M MPG Glass filled UHMW-PE
Beijing Evergrow Resources UHMW PE Fiber Rope
Mitsubishi Chemical Advanced Materials TIVAR™ 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings
Mitsubishi Chemical Advanced Materials TIVAR™ 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material

PMURT913 / 156560

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.