MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials TIVAR® Xtended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: TIVAR® Xtended Wear UHMW-PE is glass filled and partially cross-linked UHMW-PE for improved wear resistance, excellent abrasion resistance and impact strength, Low COF, No moisture abs, Corrosion resistance.

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: formerly TIVAR® Extended Wear UHMW-PE
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %<= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868ASTM D2240
Tensile Strength 38.6 MPa5600 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 300 %300 %ASTM D638
Tensile Modulus 0.421 GPa61.0 ksiASTM D638
Flexural Strength 22.8 MPa3300 psiASTM D790
Flexural Modulus 0.752 GPa109 ksiASTM D790
Compressive Strength 20.7 MPa3000 psi10% Def.; ASTM D695
Compressive Modulus 0.648 GPa94.0 ksiASTM D695
Izod Impact, Notched NBNBASTM D256 Type A
Coefficient of Friction, Dynamic 0.120.12Dry vs. Steel; QTM55007
Limiting Pressure Velocity 0.0701 MPa-m/sec2000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+10 ohm>= 1.00e+10 ohmASTM D257
Dielectric Constant 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 90.6 kV/mm2300 kV/inShort Term; ASTM D149
Dissipation Factor 0.00050
@Frequency 1e+6 Hz
0.00050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 198 µm/m-°C
@Temperature -40.0 - 149 °C
110 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.409 W/m-K2.84 BTU-in/hr-ft²-°F
Melting Point 135 °C275 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative YesYes
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters LimitedLimited
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR® SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade

P1SMP18 / 20168

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.