Sandvik Sanprint EPS is a hardened and tempered chromium steel used for printing doctor blade applications. The grade is a standard martensitic stainless steel, suitable for all types of ink and is characterized by:- Excellent wear resistance
- Good straightness
- Corrosion resistant
- Good dimensional tolerances
- Excellent edge finish
Information provided by Sandvik |