MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TriStar Ultracomp UC-200 Composite Bearing
Categories: Polymer; Thermoplastic

Material Notes: Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.

This family of composite materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of cryogenic to over 360°F with and without additional lubricants.

Ultracomp Bearing Grade Composite: Laminates composed of synthetic fabrics impregnated by thermosetting resins and solid lubricant fillers. Material is available in tubes and sheets. Ideally suited for non-lubricated ultra high-load/low-speed applications that require a low coefficient of friction. Operates well in demanding and destructive environments. Suitable for use in steam, wet, dry, or vacuum environments. Rc 35 or higher steel mating surface. Markets for Ultracomp Bearing Grade Composite include Agricultural, Appliances, Automotive, Construction, Industrial, and Transportation.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/cc
Water Absorption <= 0.10 %24 hrs
Water Absorption at Saturation <= 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100
Tensile Strength, Yield 17500 psi
Elongation at Break 26 %
Tensile Modulus 470 ksi
Flexural Strength 13500 psi
Flexural Modulus 534000 psi
Compressive Yield Strength 18500 psiPerpendicular to Laminate
 36000 psi10% deformation
Ultimate Compressive Strength 54400 psiPerpendicular to Laminate
Compressive Modulus 750 ksi
 750 ksiPerpendicular to Laminate
Ultimate Bearing Strength 54400 psiStatic Bearing
Izod Impact, Notched >= 20.0 ft-lb/in
Coefficient of Friction, Dynamic 0.15Dry vs. Steel
Coefficient of Friction, Static 0.15Dry vs. Steel
Limiting Pressure Velocity 25000 psi-ft/minUnlubricated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°FParallel to Laminate
 62.4 µin/in-°FPerpendicular to Laminate
Maximum Service Temperature, Air 266 °FContinuous
 325 °FShort Term
Minimum Service Temperature, Air -375 °FEmbrittlement Temp

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TriStar Ultracomp UC-400 Composite Bearing
TriStar Ultracomp UC-300 Composite Bearing
TriStar Ultracomp UC-500 Composite Bearing
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS
TriStar TriSteel AC Metal Backed PTFE Bearing System

PTRIST982 / 99333

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.