MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EMS-Grivory Grilamid® XE 4028 nat PA12/MACMI
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product description: Grilamid XE 4028 natural is a transparent thermoplastic polyamides based on aliphatic, cycloaliphatic and aromatic blocks. Grilamid XE 4028 natural offers a variety of interesting properties such as:
  • High transparency
  • Light and clear natural color
  • Toughness
  • Stiffness
  • FDA approved
  • Low density
  • Comfortable surface feel
  • Boiling water resistant
  • Suitable for ISBM Processes Grilamid XE 4028 is especially suitable as an alternative to Bisphenol A (BPA) containing materials, as well as for the production of optical and technical demanding parts in the application fields such as:
    • Babycare
    • Houseware
    • Packaging
    • Blow-molded containers

    Information provided by EMS Grivory.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.06 g/cc0.0383 lb/in³Dry; ISO 1183
    Water Absorption 3.5 %3.5 %Sim. to ISO 62
    Moisture Absorption 1.50 %1.50 %Sim. to ISO 62
    Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 294-4, 2577
    Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
     
    Mechanical PropertiesMetricEnglishComments
    Ball Indentation Hardness 120 MPa17400 psiConditioned; ISO 2039-1
    Tensile Strength at Break 50.0 MPa7250 psiConditioned; ISO 527-1/-2
    Tensile Strength, Yield 75.0 MPa10900 psiConditioned; ISO 527-1/-2
    Elongation at Break >= 50 %>= 50 %Nominal, Conditioned; ISO 527-1/-2
     >= 50 %>= 50 %Conditioned; ISO 527-1/-2
    Elongation at Yield 9.0 %9.0 %Conditioned; ISO 527-1/-2
    Tensile Modulus 2.20 GPa319 ksiConditioned; ISO 527-1/-2
    Charpy Impact Unnotched  NB
    @Temperature 23.0 °C
    NB
    @Temperature 73.4 °F
    Conditioned; ISO 179/1eU
     NB
    @Temperature -30.0 °C
    NB
    @Temperature -22.0 °F
    Conditioned; ISO 179/1eU
    Charpy Impact, Notched  0.700 J/cm²
    @Temperature -30.0 °C
    3.33 ft-lb/in²
    @Temperature -22.0 °F
    Conditioned; ISO 179/1eA
     0.800 J/cm²
    @Temperature 23.0 °C
    3.81 ft-lb/in²
    @Temperature 73.4 °F
    Conditioned; ISO 179/1eA
     
    Electrical PropertiesMetricEnglishComments
    Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
    Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
    Dielectric Strength 31.0 kV/mm787 kV/inConditioned; IEC 60243-1
    Comparative Tracking Index 600 V600 VConditioned; IEC 60112
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear, Parallel to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1/-2
    CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1/-2
    Maximum Service Temperature, Air 80.0 - 100 °C176 - 212 °FLong Term; ISO 2578
     120 °C248 °FShort Term; EMS
    Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FISO 75-1/-2
    Deflection Temperature at 1.8 MPa (264 psi) 130 °C266 °FISO 75-1/-2
    Glass Transition Temp, Tg 160 °C320 °F10°C/min; ISO 11357-1/-2
    Flammability, UL94 HBHBIEC 60695-11-10
     
    Optical PropertiesMetricEnglishComments
    Transmission, Visible 90 %90 %transparent; thickness not quantified
     
    Compliance PropertiesMetricEnglishComments
    FDA YesYes
     
    Descriptive Properties
    Food contactEU Requirements
     FDA
    FormGranules
    MedicalFDA
    PackagingBlow molded containers
     Injection, stretch, blow molded containers
    ProcessingExtrusion - blow molding
     Injection (stretch) blow molding
     Other Extrusion
    Special CharacteristicsTransparent

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    EMS-Grivory Grilamid® TR 55 PA12/MACMI
    Techmer ES Elastoblend® PA12 CL
    Arkema Rilsan® Clear G170 Polyamide
    Arkema Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Conditioned)
    EMS-Grivory Grilamid® TR XE 4139 black 9231 PA*

    PGRH120 / 156829

    Specialty Compounds RTP Company

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.