MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES Elastoblend® PA12 CL
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Availability: North America

Forms: Pellets

Appearance: Clear/Transparent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.011 cm/cm
@Thickness 3.17 mm
0.011 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 12 g/10 min
@Load 3.80 kg,
Temperature 230 °C
12 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 81.4 MPa11800 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Strength 98.6 MPa14300 psiASTM D790
Flexural Modulus 2.03 GPa295 ksiASTM D790
Poissons Ratio 0.400.40ASTM E132
Izod Impact, Notched 0.534 J/cm
@Thickness 3.17 mm
1.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C40.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 154 °C310 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C300 °FUnannealed; ASTM D648
Vicat Softening Point 108 °C226 °FRate B (120°C/h); ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.70 %0.70 %ASTM D1003
Transmission, Visible 90 %90 %transparent; thickness not quantified
IR Transmittance 89 - 90 %89 - 90 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® XE 4028 nat PA12/MACMI
EMS-Grivory Grilamid® TR 55 PA12/MACMI
Arkema Rilsan® Clear G170 Polyamide
Overview of materials for Nylon 12
Arkema Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Conditioned)

PTPC1047 / 136985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.