MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES Elastoblend® PA12 CL
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Availability: North America

Forms: Pellets

Appearance: Clear/Transparent

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.011 in/in
@Thickness 3.17 mm
ASTM D955
Melt Flow 12 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85ASTM D785
Tensile Strength, Yield 11800 psiASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Strength 14300 psiASTM D790
Flexural Modulus 295000 psiASTM D790
Poissons Ratio 0.40ASTM E132
Izod Impact, Notched 1.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 310 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 300 °FUnannealed; ASTM D648
Vicat Softening Point 226 °FRate B (120°C/h); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 0.70 %ASTM D1003
Transmission, Visible 90 %transparent; thickness not quantified
IR Transmittance 89 - 90 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® XE 4028 nat PA12/MACMI
EMS-Grivory Grilamid® TR 55 PA12/MACMI
Arkema Rilsan® Clear G170 Polyamide
Overview of materials for Nylon 12
Arkema Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Conditioned)

PTPC1047 / 136985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.