MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 4604 Silicone Rubber Termination Kit
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: 3M™ 4604 and 4605 Quick Term II Silicone Rubber Termination Kits are three-piece Cold Shrink terminations for Tape Shield, Wire Shield, and LC Shield power cables. They meet the requirements of IEEE standard 48-1990, for class 1 terminations. In addition they meet German standard VDE 0278 parts 5 & 100, British standard BS C-89, Spanish standard UNE 21-115-75 and Brazilian standard A-B-N-T-9314. Similar terminations using Quick Term II technology meet French EdF standards HN 33-E-01 and HN 41-E-01. Data on foreign standards are available upon request. The 3M Quick Term II consists of a high dielectric constant (High-K) stress control tube insulated with a molded silicone skirted insulator. The 4600-series termination is a twelve-skirt design incorporating in one-piece base termination assembly, a four-skirt extension insulator, and a Silicone Rubber Jacket-Sealing Cold Shrink PST Assembly. Quick Term II terminations are provided in an expanded state; mounted on a removable inner supporting plastic core. As supplied in this pre-stretched condition and termination is ready for field installation. During installation the core in unwound, allowing the termination to shrink and form a tight seal. Collectively, these termination kits cover cables with primary insulation O.D. from 1.31” to 2.60” (33 to 66 mm). These kits can be used to terminate 46 kV Shielded Power Cables from 4/0 AWG to 1500 kcm.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1200 psiSilicone Rubber Insulator; ASTM D42-68
 1394 psiEPDM Rubber Hi-K Stress Control Tube; ASTM D42-68
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.7
@Temperature 130 °C
Silicone Rubber Insulator; ASTM D150-70
 3.0
@Temperature 90.0 °C
Silicone Rubber Insulator; ASTM D150-70
 3.4
@Temperature 23.0 °C
Silicone Rubber Insulator; ASTM D150-70
 20
@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 24
@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 29
@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 35
@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 24.5
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 25.2
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 25.7
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 27.2
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 27.7
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 28.8
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
Dielectric Strength 507 kV/in
@Thickness 0.190 mm
Silicone Rubber Insulator; ASTM D149-70
Dissipation Factor 0.12
@Frequency 100000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.14
@Frequency 10000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.15
@Frequency 1000 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.16
@Frequency 150 Hz
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.093
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 0.096
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 0.132
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 400 V at 60% Strain; ASTM D150-70
 0.161
@Frequency 60.0 Hz,
Temperature 90.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.165
@Frequency 60.0 Hz,
Temperature 65.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
 0.166
@Frequency 60.0 Hz,
Temperature 23.0 °C
EPDM Rubber Hi-K Stress Control Tube, 3 kV at 60% Strain; ASTM D150-70
Track Resistance 36000 sec2.5 kV, 10 k Ohms; ASTM 2303-68

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® ST-2030 DF Polyimide
Overview of materials for Silicone Rubber
Momentive Performance Materials Silplus™ 60 CW Heat Cured Rubber - Cable & Wire
Momentive Performance Materials Silopren™ Electro 242-0 Electrically Insulating Liquid Silicone Rubber
Methanol (CH3OH; Methyl Alcohol)

PMM35163 / 169910

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.