MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cheng Yu Plastic N6GV15 Flame Retardant Nylon 6, 15% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Water Absorption 0.15 %0.15 %ASTM D570
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm0.0080 - 0.015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9494ASTM D785
Tensile Strength, Yield 129 MPa18800 psiASTM D638
Flexural Yield Strength 216 MPa31300 psiASTM D790
Izod Impact, Notched 0.873 J/cm1.63 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 224 °C435 °FASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled
RTP Company RTP 200 H FR UV Impact-Modified Nylon 6/6 (PA), High Impact - Unreinforced - Flame Retardant - UV Stabilized
RTP Company RTP 200 H FR Impact-Modified Nylon 6/6 (PA), High Impact - Unreinforced - Flame Retardant - UL94 V-0
Avient Bergamid™ AB700 UF Polyamide 66/6 Copolymer (Nylon 66/6)
Avient Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)

PLCH020 / 79168

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.