MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Cossa Polimeri ESTADIENE 2525 AS Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: ABS with high impact resistance

Good melt flow rate, with antistatic, excellent processability

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D 955
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
25 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 31.0 MPa4500 psiASTM D 638
Tensile Strength, Yield 37.0 MPa5370 psiASTM D 638
Elongation at Break 20 %20 %ASTM D 638
Flexural Modulus 2.50 GPa363 ksiASTM D 790
Izod Impact, Notched  2.00 J/cm
@Temperature 0.000 °C
3.75 ft-lb/in
@Temperature 32.0 °F
ASTM D 638
 2.50 J/cm
@Temperature 23.0 °C
4.68 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  93.0 °C
@Load 5.00 kg
199 °F
@Load 11.0 lb
50°C/hr; ASTM D 1525
 101 °C
@Load 0.999 kg
214 °F
@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Test 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
I.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
Aclo Accucomp ABS ABS802L High Impact Grade
Covestro Desmopan® 588 Thermoplastic Polyurethane
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced

PCOSSA825 / 156415

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.