MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poly-u-Mac Air-Cell T-50 Polyester Foam Core
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Air-Cell is a hybrid, closed cell cross-linked polyester foam core that is an economical alternative to other cores used in the production of sandwich composite structures. In addition to its excellent strength to weight ratio, it offers good dimensional stability at elevated temperatures. Aircell T grade is available in a wide range of densities in order that designers, engineers and fabricators can select the most appropriate density for the prevailing application. It is suitable for a wide range of marine, road/rail transportation, aerospace and industrial applications. Poly-U-Mac offers a comprehensive kitting service for the Air-Cell product line with the capability to work directly from customers' CAD files. Used 'straight out of the box', Poly-U-Mac Air-Cell kits speed the manufacturing process, save labor costs and virtually eliminate material waste.

Key Features:

  • High strength to weight ratio
  • Good dimensional stability
  • Can be processed at up to 200°F
  • High 'in service' temperature performance
  • Does not absorb water
  • Compatible with most resins (polyester, epoxy and vinylester systems)
Typical Applications
  • Leisure & Commercial Marine: hulls, decks, stringers & bulkheads
  • Wind Energy: blades, cabins & spinners
  • Road: cabs, sleeper floors & RV bodies
  • Rail: train fronts, floors, cabs, exterior & interior paneling
  • Aerospace: flooring, toilet modules & overhead lockers

Information provided by Poly-u-Mac

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0681 - 0.0881 g/cc0.00246 - 0.00318 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.32 MPa191 psiASTM D1623
Flexural Strength 1.19 MPa172 psiASTM D790
Compressive Strength 0.814 MPa118 psiASTM D1621
Compressive Modulus 0.02252 GPa3.266 ksiASTM D1621-B
Poissons Ratio 0.300.30
Shear Modulus 0.009556 GPa1.386 ksiASTM C273
Shear Strength 0.621 MPa90.0 psiASTM C273
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°F
Maximum Service Temperature, Air 73.9 °C165 °F
Minimum Service Temperature, Air -196 °C-320 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 93.3 °C<= 200 °F
 
Descriptive Properties
Water Absorption0.063 lb/ft2ASTM D2842

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Calcium Carbonate, Calcite (CaCO3)
Aluminum 6061-O
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Kolon KOPA® KN333HB30BL Hybrid Nylon 66
Magnesium, Mg; Annealed Sheet

PPUMC001 / 186876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.