MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Cold Rolled
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to achieve weight savings of 30% to 50% compared to conventional cold forming grades. The main advantages of Usibor® 1500 and 22MnB5 are:
  • Ability to achieve complex geometry in both the direct process (forming in austenitic state) and the indirect process (good cold formability). Their very good hot formability makes it possible to offer steel solutions that integrate several functions (elimination of reinforcement parts and assemblies);
  • Total absence of springback;
  • Uniform mechanical properties obtained on the part;
  • Exceptional fatigue strength (Usibor® 1500) and impact resistance, allowing substantial weight reduction. ArcelorMittal was the first steelmaker to deliver a coated press hardened steel, Usibor® 1500-AS with an aluminum-silicon coating.
The additional advantaes of Usibor® 1500-AS, above and beyond those of 22MnB5, are:
  • Simplified process and cost savings: elimination of the shot-blasting step (no formation of scale), no need for protective atmosphere in austenitization ovens;
  • Excellent temporary corrosion resistance after stamping, no need to oil parts before assembly;
  • No decarburization;
  • Excellent resistance to pitting corrosion, currently used in dry and wet areas (e.g. side sill) of the vehicle.
Usibor® 1500-GI galvanized Zn (for indirect stamping process only) and Usibor® 1500-GA galvannealed ZnFe (for both direct and indirect processes) now round out the coating offer. ArcelorMittal has now added the Ductibor® 500 grade to its range. This product is offered in association with Usibor®1500 in Laser Welded Blank (LWB) solutions that locally provide more ductile properties than those of Usibor® 1500. This makes it possible to precisely control the crash deformation of specific vehicle parts (e.g. B-pillar reinforcement) and expands the use of hot stamping steels to energy absorption parts (e.g. front or rear rail).

Applications:Usibor® 1500 and 22MnB5 are particularly well suited for the entire range of structural parts requiring good crash resistance. Current applications include:

  • Front and rear bumper beams;
  • Door reinforcements;
  • Windscreen upright reinforcements;
  • B-pillar reinforcements;
  • Floor and roof reinforcements;
  • Roof and dash panel cross members.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 500 - 700 MPabefore hot stamping
 1500 MPaafter hot stamping
Tensile Strength, Yield 320 - 550 MPabefore hot stamping
 1100 MPaafter hot stamping
Elongation at Break 6.0 %after hot stamping, L0=80 mm, th<3 mm
 >= 10 %before hot stamping, L0=80 mm, th<3 mm
Fatigue Strength 305 MPa
@# of Cycles 2.00e+6
σD A, R=1
 617 MPa
@# of Cycles 2.00e+6
σD A, R=0.1
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.25 %
Iron, Fe >= 98 %as balance
Manganese, Mn <= 1.4 %
Silicon, Si <= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Hot Rolled
ArcelorMittal Usibor® 1500 Ultra high strength steel, Hot Rolled
Ovako 22MnB5 Steel
ArcelorMittal MartINsite® 1200 Cold Rolled Steel
ArcelorMittal Usibor® 1500 Ultra high strength steel, Cold Rolled

NARCE004 / 159912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.