MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovako 22MnB5 Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Grade SB24M13B is a boron steel for general purposes without any specified mechanical properties. Its closest equivalent is found in the standard number 22MnB5.This grade is suitable to serve as chains (side-links) in materials handling equipment of various kinds that are exposed to heavy wear and varying stresses (bending, tensile, fatigue). This grade also works well as wear parts in snow ploughs/graders and in the machinery of agriculture machines because of its good hardness and toughness in heat-treated condition in dimensions up to Ø 40 mm or equivalent thickness.

Information provided by Ovako

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 400 °C752 °FMS
 719 °C1330 °FAC1
 790 °C1450 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.00080 - 0.0050 %0.00080 - 0.0050 %
Carbon, C 0.19 - 0.25 %0.19 - 0.25 %
Chromium, Cr <= 0.40 %<= 0.40 %
Iron, Fe 97.51 - 98.71 %97.51 - 98.71 %As Balance
Manganese, Mn 1.1 - 1.4 %1.1 - 1.4 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.015 %<= 0.015 %
 
Descriptive Properties
WeldabilityCEV 0.52max
 Pcm 0.33max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Hot Rolled
ArcelorMittal Usibor® 22MnB5 Ultra high strength steel, Cold Rolled
Ovako 22MnB5 SB24M13B Steel
ArcelorMittal Usibor® 1500 Ultra high strength steel, Cold Rolled
ArcelorMittal Dual Phase 980 LCE Y600 Very High Strength Cold Rolled Steel

NOVAKO174 / 234473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.