MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: 25 wt% Vinyl Acetate.

Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.

Additives: Antioxidant.

Applications: Elvax® 3190 is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. Elvax® 3190 is also available in a "Low Gel" version (Elvax® 3190LG) for applications requiring superior film quality. The melt properties of this resin allow it to be processed on blown or cast coextrusion film equipment over a wide range of line speeds and film thicknesses. It can be coextruded with a variety of other polymers. Elvax® 3190 is typically used as a low temperature seal layer in coextruded film.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Viscosity 1.00e+6 cP
@Shear Rate 50 1/s,
Temperature 190 °C
estimated from log-log graph
Melt Flow 2.0 g/10 minCondition not noted.; ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 55.0 °CFreezing Point via DSC/ASTM D3418
 77.0 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 52.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 175 - 215 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvax® 3180Z Ethylene Vinyl Acetate
Dow Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
DuPont Elvax® 4355 Ethylene Vinyl Acetate
Dow Elvax® 3175 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
Dow Elvax® 3176 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Extrusion Coating

PDUPHN / 33626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.