MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Elvax® 3176 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Extrusion Coating
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: 18 wt% Vinyl Acetate.

Elvax® 3176 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.

Additives: Slip, Chill Roll Release, Antioxidant.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Melt Flow 30 g/10 min30 g/10 minCondition not noted.; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.170.17coating/coating; ASTM D1894
 0.430.43coating/metal; ASTM D1894
 
Thermal PropertiesMetricEnglishComments
Melting Point 65.0 °C149 °FFreezing Point via DSC/ASTM D3418
 87.0 °C189 °FUpon Melting via DSC/ASTM D3418
Vicat Softening Point 54.0 °C129 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 232 °C392 - 450 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 3180Z Ethylene Vinyl Acetate
Dow Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
Dow Elvax® 3182 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
Dow Elvax® 3124 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
Dow Elvax® 3182-2 Ethylene Vinyl Acetate

PDUPHL / 33624

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.