MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Unifrax FyreWrap® EZ 1.5 Duct Insulation Ventilation Air Duct (VAD) System
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Unifrax's FyreWrap® EZ 1.5 Duct Insulation is a new optimized single-layer flexible enclosure for 1- and 2-hour fire-rated ventilation air ducts (VAD). Typical duct types include smoke control, stairwell and vestibule pressurization, ventilation, heating and air conditioning supply/return, and commercial dryer exhaust, as well as refuse and linen chutes. This slim, compact design is an alternate to code prescribed fire-rated shafts and results in significant weight, space and labor savings when compared to traditional shafts. FyreWrap EZ 1.5 Duct Insulation VAD System offers the following features:

  • 1- and 2-hour fire-rated enclosure
  • Zero clearance to combustibles at all locations on blanket wrap
  • Alternate to fire-rated shaft
  • Saves weight, space, labor
  • Thin, lightweight single-layer system
  • High-temperature, biosoluble insulation
  • Durable foil-scrim covering
  • GREENGUARD listed for Microbial Resistance

    Product Components
  • Core Material: FyreWrap EZ 1.5 Duct Insulation incorporates Insulfrax® Thermal Insulation as its core material. Insulfrax is a high-temperature insulation made from calcia, magnesia, silica chemistry designed to enhance biosolubility. It provides excellent insulation in a noncombustible blanket form.
  • Encapsulating Material: The core insulation is completely encapsulated in an aluminum foil, fiberglass-reinforced scrim covering. This scrim provides additional handling strength as well as protection from tearing and moisture absorption.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.00 lb/ft³
Thickness 1500 mil
 
Thermal PropertiesOriginal ValueComments
Insulation R Value 6.19ASTM C518
 
Descriptive Properties
ASTM C136 Non-combustibilityPass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Ventilation Air Duct (VAD) System
Wacker Wetsoft® NE 230 Silicone Softener Emulsion
Silicon, Si
Goodfellow Reaction Bonded Silicon Carbide SiC
CHT Group QM 263 60 Shore A, Inhibition Resistant, Addition Cure Moldmaking Material

CUNIF114 / 97886

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.