Unifrax's FyreWrap® EZ 1.5 Duct Insulation is a new optimized single-layer flexible enclosure for 1- and 2-hour fire-rated ventilation air ducts (VAD). Typical duct types include smoke control, stairwell and vestibule pressurization, ventilation, heating and air conditioning supply/return, and commercial dryer exhaust, as well as refuse and linen chutes. This slim, compact design is an alternate to code prescribed fire-rated shafts and results in significant weight, space and labor savings when compared to traditional shafts. FyreWrap EZ 1.5 Duct Insulation VAD System offers the following features:- 1- and 2-hour fire-rated enclosure
- Zero clearance to combustibles at all locations on blanket wrap
- Alternate to fire-rated shaft
- Saves weight, space, labor
- Thin, lightweight single-layer system
- High-temperature, biosoluble insulation
- Durable foil-scrim covering
- GREENGUARD listed for Microbial Resistance
Product Components- Core Material: FyreWrap EZ 1.5 Duct Insulation incorporates Insulfrax® Thermal Insulation as its core material. Insulfrax is a high-temperature insulation made from calcia, magnesia, silica chemistry designed to enhance biosolubility. It provides excellent insulation in a noncombustible blanket form.
- Encapsulating Material: The core insulation is completely encapsulated in an aluminum foil, fiberglass-reinforced scrim covering. This scrim provides additional handling strength as well as protection from tearing and moisture absorption.
Information Provided by Unifrax I LLC |