PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surface just prior to the molding of SMC/BMC. Applications can be found in sanitary products such as kitchen sinks and shower trays. A special, appealing color effect is created by mixing different colors, which gives a speckle effectInformation provided by Raschig Group |