MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Raschig Group PiMC 1249 Sanitary, mix color
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surface just prior to the molding of SMC/BMC. Applications can be found in sanitary products such as kitchen sinks and shower trays. A special, appealing color effect is created by mixing different colors, which gives a speckle effect

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 - 1.50 g/cc1.30 - 1.50 g/cc
Bulk Density 0.600 - 0.700 g/cc0.0217 - 0.0253 lb/in³
Particle Size 10 - 25 µm10 - 25 µmD 0.1, SATP-114, Malvern method
 50 - 75 µm50 - 75 µmD 0.5, SATP-114, Malvern method
 100 - 175 µm100 - 175 µmD 0.9, SATP-114, Malvern method
Storage Temperature <= 20.0 °C<= 68.0 °F
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 2.0 - 5.0 %2.0 - 5.0 %ASTM D790
Flexural Strength 30.0 - 60.0 MPa4350 - 8700 psiASTM D790
Flexural Modulus 5.00 - 10.0 GPa725 - 1450 ksiASTM D790
Abrasion <= 0.50
@Load 0.500 kg
<= 0.50
@Load 1.10 lb
[g] S42 paper, 500 turns; DIN 53799
 
Optical PropertiesMetricEnglishComments
Gloss 50 %50 %20°
 75 %75 %60°
 90 %90 %85°
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Barbender cycle time75-115 s150°C, SATP-104
Powder stability>8 hrs30°C, SATP-128
Scratch resistance>2 NDIN 53799

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRASCI33 / 179170

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.