MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Material Notes: Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release.

Features: Good Mold Release; Good Thermal Stability; Good Surface Finish; High Gloss

Processing Method: Injection Molding

Forms: Pellets

Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure; High; Injection Rate: Moderate

Resin ID (ISO 1043): PBT+PET-GF 15

Information Provided by Teknor Apex

Key Words: PET, PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 482 - 536 °F
Middle Barrel Temperature 482 - 536 °F
Front Barrel Temperature 482 - 536 °F
Melt Temperature <= 500 °FProcessing Temperature
Mold Temperature 266 - 302 °F
Drying Temperature 248 °F
Dry Time 4 hour
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Biomax® TPS 2501
Teknor Apex Terraloy™ MB 20001A Thermoplastic Starch + Copolyester
DuPont Biomax® TPS 2100
Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp
Celanese Zytel® 151 NC010 PA612

PTEKNO446 / 128623

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.