MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Lupolen 4261A Q135 High Density Polyethylene (HDPE), Extruded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Lupolen 4261A Q135 is a high molecular weight high density polyethylene. Typical customer applications include automotive fuel tank applications. It is supplied in powder form and is stabilized with antioxidants for the extrusion process. The product features an outstanding Environmental Stress Cracking Resistance (ESCR), good chemical resistance in combination with an excellent low temperature impact resistance. Typical processes include blow molding and thermoforming. Lupolen 4261A Q135 is not intended for use in medical and pharmaceutical applications. Applications: Fuel Tanks

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.490 g/cc>= 0.0177 lb/in³ISO 60
Density 0.945 g/cc0.0341 lb/in³ISO 1183-1
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourcond. B, 10% Arkopal; ASTM D1693
Melt Flow 6.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.0 MPa3480 psiISO 527-1,-2
Elongation at Yield 10 %10 %ISO 527-1,-2
Tensile Modulus 0.900 GPa131 ksiISO 527-1,-2
Tensile Impact Strength 170 kJ/m²
@Temperature -30.0 °C
80.9 ft-lb/in²
@Temperature -22.0 °F
notched, type 1, method A; ISO 8256
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FISO 3146
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °F
 
Descriptive Properties
FNCT (hrs)80ISO 16770, 3.5 MPa, 2% Arkopal N100, 80°C
Processing MethodExtrusion Blow Molding, Thermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® LR732031 High Density Polyethylene
LyondellBasell Lupolen 4552D BLACK High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG UV60005 High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG UV High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG Q469 High Density Polyethylene (HDPE), Extruded

PEQT8564 / 220199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.