MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Lupolen 4261AG UV60005 High Density Polyethylene (HDPE), Extruded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Lupolen 4261AG UV60005 is a high density polyethylene with outstanding ESCR, high impact resistance and good chemical resistance. It is delivered in pellet form and contains antioxidants and a UV-stabilizer. Typical customer applications include Intermediate Bulk Containers (IBC) for the packaging of dangerous goods and heating oil tanks. Lupolen 4261AG UV60005 is not intended for use in medical and pharmaceutical applications. Applications: Heating Oil Tanks, Industrial Packaging, Intermediate Bulk Containers

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³ISO 60
Density 0.945 g/cc0.0341 lb/in³ISO 1183-1
Viscosity Test 370 cm³/g3.70 dl/gIntrinsic; ISO 1628-3
Melt Flow  0.35 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.35 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 6.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 40.0 MPa5800 psiISO 2039-1
Tensile Strength, Yield 24.0 MPa3480 psiISO 527-1,-2
Elongation at Yield 10 %10 %ISO 527-1,-2
Tensile Modulus 0.850 GPa123 ksiISO 527-1,-2
Tensile Impact Strength 170 kJ/m²
@Temperature -30.0 °C
80.9 ft-lb/in²
@Temperature -22.0 °F
notched, type 1, method A; ISO 8256
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °Funannealed; ISO 75B-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C108 °Funannealed; ISO 75A-1,-2
Vicat Softening Point 75.0 °C167 °FB50; ISO 306
 125 °C257 °FA50N; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °Fblow molding process
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 132/30
FNCT (hrs)60ISO 16770, 3.5 MPa, 2% Arkopal N100, 80°C
Processing MethodExtrusion Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 4261AG BD High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG UV High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG Q474 High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen 4261AG Q469 High Density Polyethylene (HDPE), Extruded
LyondellBasell Lupolen 4261AG High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

PEQT8561 / 220196

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.