Sil-O-Wet® grades are leafing and non-leafing aluminum pigment pastes carried in isopropyl alcohol in which the aluminum flakes have been chemically treated to reduce the aluminum-water reaction. These grades are recommended for use in aqueous flexographic and gravure ink formulations. The specific degree of gassing stability is formulation dependent and each formulation must be evaluated for acceptable stability. High or excessive shear during processing will reduce the effectiveness of the inhibitor and should be avoided. Applications: Printing Inks; Waterborne |